Aluminum alloy welding wire is specialized in production pure aluminum welding rod, aluminum magnesium welding rod, aluminum silicon welding rod, low silicon welding rod, high silicon welding rod.The aluminum welding wires are widely used in bicycles, aluminium scoter, engine carriage, pressure vessel, armary processing, ship-building, space shuttle etc.
AWS A 5-10 Data | ER1060 | ER1100 | ER2319 | ER4043 | ER4047 | ER5356 | ER5183 | ER5556 |
Typical composition in% | Si | <0.25 | Si+Fe<0.95 | <0.20 | 4.50-5.50 | 11.00-13.00 | <0.25 | <0.40 | <0.25 |
Fe | <0.35 | <0.30 | <0.80 | <0.60 | <0.40 | <0.40 | <0.40 |
Cu | <0.05 | 0.05-0.20 | 5.80-6.80 | <0.30 | <0.30 | <0.10 | <0.10 | <0.10 |
Mn | <0.03 | <0.05 | 0.20-0.40 | <0.05 | <0.15 | 0.05-0.20 | 0.50-1.00 | 0.60-1.00 |
Mg | <0.03 | - | <0.02 | <0.05 | <0.10 | 4.50-5.50 | 4.30-5.20 | 4.70-5.50 |
Cr | - | - | | | | 0.05-0.20 | 0.05-0.25 | 0.05-0.20 |
Zn | <0.05 | <0.10 | <0.10 | <0.10 | <0.20 | <0.10 | <0.25 | <0.20 |
Be | - | <0.0008 | <0.0003 | <0.0003 | <0.0003 | <0.0003 | <0.0003 | <0.0003 |
Ti | <0.03 | - | 0.10-0.20 | <0.20 | <0.15 | 0.06-0.20 | <0.15 | 0.05-0.20 |
Physical properties(Approx. Values) | 0.2% yield strength Rp0.2 Mpa | 20 | 25 | 180 | 40 | 60 | 110 | 125 | 125 |
Tensile strength Rm Mpa | 65 | 80 | 240 | 120 | 130 | 240 | 275 | 275 |
Elongation A5(L0=5d0) % | 18 | 25 | Ca.3 | 8 | 5 | 17 | 17 | 17 |
Test temperature ℃ | 20 | 20 | 20 | 20 | 20 | 20 | 20 | 20 |
Specifications: MIG-wires, 0.8mm,0.9mm,1.0mm,1.2mm,1.6mm2.0mm,2.4mm
TIG-rods, 1.6mm,2.0mm,2.4mm,3.2mm,4.0mm,5.0mm, 6.0mm
MIG Packing:0.5kg, 1kg,2kg, 6kg, 7kg/plastic spool
TIG Packing: 5kg, 10kg per paper box or plastic box, Length 1.000mm
Notice of usage and storage
1 You can do welding directly in effect without any processing before welding after opening the box of products,The products will be in effect more than two years on condition they are of good packing in seal.
2 The products should be put to the place where is of aeration and dryness and away from the medium of acidalkalioil and so on.
3 The products should be avoided of crack and damp during delivery so as to avoid destroying the welding spools and impacting the quality of welding wires.
4 We suggest you to put some dust-proof on the surface of wires after the packages are moved from the products.
5 We suggest you to do some processing to the surface of the wires before welding when you use the wires out of storage life.
6 The arc welding may hurt your eyes during welding. please protect yourself.